Notes: Telcar TL-2580F is a general purpose thermoplastic elastomer designed for a variety of industrial applications. Telcar TL-2580F is a high density, high hardness grade suitable for both injection molding and extrusion. Features: Filled; General Purpose; Good Colorability; High Density; High Flow; High Specific Gravity; High Hardness; Oil Extended Uses: General Purpose; Grommets; Industrial Applications; Industrial Parts; Rubber Replacement Form: Pellets Processing Method: Injection Molding; Extrusion Injection Notes: Injection Rate: Moderate-Fast Extrusion Notes: Screw Speed: 30 to 100 rpm Information Provided by Teknor Apex |