MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Polimersan Plastics POLIKES® (PA 6 G) Cast Polyamide
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Cast

Material Notes: POLIKES® PA6 G (CAST POLYAMIDE) is a plastic with high physical, electrical and chemical resistance. Its resistance is high especially against strokes and loads. Its temperature resistance is high, whereas corrosion coefficient is low. But, because of its water absorption property, it is not recommended at humid environments(%6-7).

PROPERTIES OF POLIKES®:

  • 100°C Service Temperature
  • Low Corrosion Coefficient
  • Very High Pressing Resistance
  • High Hardness
  • High Resistance To Strokes
  • Resistance To Heat
  • Resistance To Chemical Substances
  • Lower Water Absorption compared to PA 6
GENERAL USAGE AREAS OF POLIKES®:
  • Sledges
  • Wheels
  • Rolls
  • Gears
  • Bearings
  • Bobbins
  • Hoops
  • Corrosion Plates
  • Food Industry Parts
  • Chemical Industry Parts
  • Paper Industry Parts
  • Textile Industry Parts
  • Press Industry Parts

Information provided by Polimersan Polimer Kimya San.Tic.Ltd.Sti.

Vendors:
Available Properties
  • Specific Gravity, ISO.1183 DN.53479
  • Water Absorption, ISO.62 DN.53495
  • Hardness, Rockwell M, ISO.2039-2
  • Hardness, Shore D, DN.53505
  • Ball Indentation Hardness, ISO.2039-2
  • Tensile Strength at Break, ISO.527 DN.53455
  • Tensile Strength, Yield, ISO.527 DN.53455
  • Elongation at Break, ISO.527 DN.53455
  • Modulus of Elasticity, ISO.178 DN.53452
  • Volume Resistivity, ISO.167 DN.53482
  • Surface Resistance, ISO.167 DN.53482
  • Dielectric Strength, ISO.243 DN.53481
  • CTE, linear, DN.53752
  • Melting Point
  • Maximum Service Temperature, Air, ISO.75 DN.53461
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic
PA, Polyamide

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.