MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Evonik Rohacell® 150 EC Electrically Conductive Grade Polymethacrylimide (PMI) Foam
Categories: Other Engineering Material; Composite Core Material; Polymer; Thermoset; Polymethacrylimide

Material Notes: ROHACELL® EC is a polymethacrylimide (PMI) based foam core material specifically designed for stealth applications. During processing, the polymer is loaded with carbon particles resulting in a conductive foam product that possesses superior dielectric properties and enables absorption of electromagnetic waves at radar frequencies.

Due to its closed cell structure, ROHACELL® EC provides controlled resin absorption since the resin enters only the cut cells on the surface of the core material. This assures secure bonding of the core to the surface layers, but adds no excessive resin weight to the finished part.

Replaces Rohacell® 150EC-4.

Information provided by Evonik Industries.

Vendors:
Available Properties
  • Density, DIN 53420, ISO 845, ASTM D 1622
  • Tensile Strength at Break, DIN 53455, ISO 527-2, ASTM D 638
  • Modulus of Elasticity, ISO 527-2, ASTM D 638
  • Compressive Strength, DIN 53421, ISO 844, ASTM D 1621
  • Poissons Ratio, Calculated
  • Shear Modulus, DIN 53294, ASTM C 273
  • Shear Strength, DIN 53294, ASTM C 273
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Evonik Corporation (Former Evonik Degussa GmbH)

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.