MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Magnesium ZK61A-T5, Cast
Categories: Metal; Nonferrous Metal; Magnesium Alloy

Material Notes: Typically used for simple, highly stressed aerospace and military castings of uniform cross section. High in cost. Intricate castings subject to microporosity and cracking due to shrinkage. Not readily welded. Sometimes used in T5 temper (artificially aged), but usually in the solution heat treated and artificially aged (T6) condition to develop properties fully.

Key Words: UNS M16611; Mg; AMS 4444; ASTM B 80; SAE J465; Old SAE 513 (Ingot UNS M16610)
Vendors:
Available Properties
  • Density
  • Hardness, Brinell, 500 kg load, 10 mm ball
  • Hardness, Knoop, Estimated from Brinell
  • Hardness, Vickers, Estimated from Brinell
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break, in 50 mm
  • Tensile Modulus, Typical Mg alloy
  • Compressive Yield Strength, at 0.2% offset
  • Poissons Ratio, Estimated from similar Mg alloys.
  • Machinability, Relative Rating, 100=Best
  • Shear Modulus, Estimated from similar Mg alloys.
  • Shear Strength
  • Electrical Resistivity, Estimated from trends in similar alloys.
  • Heat of Fusion, Estimated from trends in similar Mg alloys.
  • CTE, linear
  • CTE, linear
  • Specific Heat Capacity
  • Thermal Conductivity, Estimated from trends in similar Mg alloys.
  • Melting Point
  • Solidus
  • Liquidus
  • Casting Temperature, Sand Casting
  • Copper, Cu
  • Magnesium, Mg, As remainder
  • Nickel, Ni
  • Other, total
  • Zinc, Zn
  • Zirconium, Zr
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.