MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
DAK Americas Laser+® MB912 PET
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); Polyethylene Terephthalate (PET), Unreinforced

Material Notes: Product Description: Laser+® MB912 polymer is a polyethylene terephthalate resin designed specifically for the carbonated soft drink (CSD) and other beverage markets. It delivers fast, efficient processing and good overall bottle properties. This polymer is formulate to provide improved efficiencies in perform and bottle production while delivering a robust processing window. Bottles made with Laser+® MB912 deliver good CO2 barrier with continued excellent performance in creep and environmental stress-crack resistance.

Key Attributes:

  • Good performance in stress-crack resistance
  • High reheat capability that provides fast and efficient processing in stretch blow molding
  • Good CO2 barrier
  • Robust processing window

Application/Uses: Carbonated soft drink bottles and custom, edible oil, food, juices and personal care bottles and containers.

Information provided by DAK Americas

Vendors:
Available Properties
  • Bulk Density, ASTM D1895, Poured
  • Bulk Density, ASTM D1895, Vibrated
  • Density, ASTM D1505, Crystalline
  • Melt Density, ASTM D1238
  • Particle Size, Cubical Shape
  • Viscosity Test, DRAM-A-G-V-3, Intrinsic
  • Heat of Fusion, ASTM E793, DSC on the first heating cycle
  • Specific Heat Capacity, ASTM E1269
  • Specific Heat Capacity, ASTM E1269
  • Specific Heat Capacity, ASTM E1269
  • Specific Heat Capacity, ASTM E1269
  • Specific Heat Capacity, ASTM E1269
  • Crystallization Temperature, ASTM D3418, DSC on second heating cycle, Peak Melting Point
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.