Hostacom BE17FC BLK fractional melt flow, 1,800 MPa flexural modulus, UV stabilized, precolored, 40% Calcium Carbonate filled polypropylene copolymer is typically used for a variety of extrusion and blow molding applications. It is characterized by an excellent overall balance of properties. Applications: Automotive Parts, Exterior Automotive Applications, Under hood.Information provided by LyondellBasell. |