Composition: ADOGEN® 66 is 100 % Ethyl bis-(polyethoxyethanol) tallow ammonium ethosulfate. Application field: - ADOGEN® 66 quat is most commonly used as an antistatic agent, effective on cellulosic and synthetic fibers and fabrics.
- Water soluble, cationic surfactant, suggesting uses as a dispersing agent, dye retarder, and general purpose emulsifier.
- Application rates at levels of 0.05 % -0.1 % based on fiber or fabric weight give demonstrable reductions in static charges.
Benefits:- Effective antistatic agent on polyester, nylon and acrylic fabrics
- Very good thermal stability
- Highly hydrophilic quaternary ammonium compound
- Viscous liquid, free of solvents, non chloride salt
- Non corrosive
- Compatible with anionic surfactants with out salt precipitation
Information provided by Evonik |