MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Dow Bynel® 4157 Adhesive Resin
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate

Material Notes: Bynel® Series 4100 resins are anhydride-modified linear low-density polyethylene (LLDPE) resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyethylene (PE) resins.

Applications:Bynel® Series 4100 resins adhere to a variety of materials. They are most often used to adhere to EVOH, polyamide, PE, ionomers, and ethylene copolymers.

Bynel® Series 4100 resins can be used in coextrusion processes including:

  • blown film
  • cast film/sheet
  • blow molding melt and solid phase thermoforming
  • sheet and tubing
  • Bynel® 4157 can also be used in coextrusion coating. LLDPE resins are known for their temperature resistance, clarity and toughness. These physical properties make the Bynel® Series 4100 resins work well in applications such as:

  • boil-in-bag structures
  • blow molded containers in which drop strength is important
  • bag-in-box films
  • film where LLDPE is the heat seal layer

    Information provided by DuPont™

    This former DuPont product line is now a Dow product line.

  • Vendors:
    Available Properties
    • Density, ASTM D792
    • Melt Flow, ASTM D1238
    • Melting Point, ASTM D3418, Freezing Point, DSC
    • Melting Point, ASTM D3418, DSC
    • Vicat Softening Point, ASTM D1525
    • Rear Barrel Temperature, For high temperature coextrusions.
    • Rear Barrel Temperature, For coextrusion with EVA or EVOH.
    • Middle Barrel Temperature, For coextrusion with EVA or EVOH.
    • Middle Barrel Temperature, For high temperature coextrusions.
    • Front Barrel Temperature, For coextrusion with EVA or EVOH.
    • Front Barrel Temperature, For high temperature coextrusions.
    • Adapter Temperature, For coextrusion with EVA or EVOH.
    • Adapter Temperature, For high temperature coextrusions.
    • Die Temperature, For coextrusion with EVA or EVOH.
    • Die Temperature, For high temperature coextrusions.
      
    Property Data

    This page displays only the text
    of a material data sheet.

    To see MatWeb's complete data
    sheet for this material (including
    material property data, metal
    compositions, material suppliers,
    etc
    ), please click the button below.

    Manufacturer Notes:
    Dow Chemical (former DuPont)

    Category Notes
    Plastic

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

     

    Rulon Bearings
    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.