MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
NRI Composite Guard™ FP Composite Fire Proofing System
Categories: Other Engineering Material; Composite Core Material

Material Notes: Description: NRI’s Composite Guard™ FP system utilizes nano-technology to create an integrated fire proofing system for application on high risk piping within fire proofing zones in refineries and on offshore platforms. The Composite Guard FP System protects the composite repair under extreme fire conditions by creating a barrier between the external flame temperature and the composite repair’s outer substrate. The extremely low thermal conductivity of the barrier prevents the composite repair system from reaching temperatures exceeding the maximum temperature rating, preventing degradation or failure of the composite.

Typical Applications:

  • Offshore platforms
  • Refineries
  • Chemical processing plants
Benefits:
  • Increase safety
  • Designed specifically for use with composite repairs
  • Fast Installation
  • Lightweight
  • Impact resistant
  • Long term durability
  • Provides instant fire protection
  • Does not require flame exposure to form a thermal barrier like other coatings

Information provided by NRI® Innovative Composite Solutions

Vendors:
Available Properties
  • Compressive Strength, ASTM C165
  • Compressive Strength, ASTM C165
  • Maximum Service Temperature, Air, ASTM C447, Estimated, Use
  • Maximum Service Temperature, Air
  • Shrinkage, Linear Shrinkage Under Soaking Heat
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.