9 wt% Vinyl Acetate. Elvax® 3124 is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins. Additives: Antioxidant Applications: Elvax® 3124 is designed to provide a low-temperature heat seal to itself or many other materials commonly used in flexible packaging applications. The melt properties of this resin allow it to be processed on extrusion coating equipment over a wide range of line speeds and coating thicknesses. It can also be coextrusion coated with a variety of other polymers. Information provided by DuPont Packaging Polymers. This former DuPont product line is now a Dow product line. |