MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Wacker Silres® K Silicone Resin
Categories: Polymer; Thermoset; Silicone

Material Notes: Product description: SILRES® K is a solution of a methyl silicone resin in toluene. The silicone resin itself has a very high concentration of SiO2 (after complete oxidation: approx. 80% SiO2, expressed in terms of solid resin [DSC]). It is therefore an ideal binder for applications where temperatures exceed 300°C. As SILRES® K evolves less smoke and offers greater binding strength, it is much superior to phenyl silicone resins.

Special features:

  • 80% SiO2 content, expressed in terms of solid resin
  • high binding strength
  • little smoke evolution on pyrolysis
  • excellent thermal stability
Application: By virtue of its high SiO2 content, SILRES® K is the standard binder for the production of rigid, silicone resin-bound mica insulators and compression molding compounds for electrical engineering. SILRES® K is also an excellent binder for mica splitting.

Information provided by Wacker Chemie AG.

Vendors:
Available Properties
  • Density, DIN 51757
  • Kinematic Viscosity, DIN 51562
  • Flash Point, DIN 51755
  • Ignition Temperature, EN 14522
  • Transmission, Visible, "Clear" but manufacturer does not quantify.
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.