Features Modified homopolymer PP for injection moulding with the content of 40% microground, floated, chemically modified talc.Contains modificator for laser labeling of finisched parts. /LASER NdIAG - 1064nm/. Application in automotive industry.Covers of car chassis, fenders, motors etc. Delivered in black mode. Packaging, transport, stocking The product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.000 kg palette, in paper octabins with a thick PE foil fixed on a 1.000 kg palette or in other packaging according to customer requirements. The transport is provided in closed-up vehicles where the material is protected against movement and mechanical damage. The product requires stocking in closed-up, dry places protected against sun and thermal radiation. Information Provided by Plastcom spol. s r.o. |