MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Schott Sapphire Optical Window
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: Sapphire, as one of the hardest, most durable and scratch resistant materials, offers a broad transmission range from UV to mid infrared wavelengths (250 – 5000 nm). It is able to withstand extreme environmental conditions and temperature changes. SCHOTT offers sapphire windows in different supply forms, dimensions, and in customized processing stages.Material:
  • Extreme hardness & high mechanical strength (withstands extreme environmental conditions)
  • Excellent thermal conductivity/heat resistance
  • High transmittance (UV to IR)
  • Low dn/dT
  • High electrical resistance (10e14 Ohm-cm)
  • High dielectric constant (9.39 from 1.0 MHz to 8.5 GHz)
Applications:
  • Infrared applications (e. g. radiometry, guidance, gas analysis, medicine, safety and security)
  • High-pressure and shock-loading applications (e.g. chamber or heater windows in chemical process equipment)
  • Optical applications (e.g. optical components from UV to IR)
  • Scratchproof sapphire watch glasses
Advantages:
  • SCHOTT offers sapphire material in optical quality
  • Customized characteristics concerning dimensions and shapes (round, square, and more, diameters up to 300 mm)
  • Polished surface and customized coating for different applications
  • Best Practice in sapphire processing due to long term experiences from handling optical materials
  • Usage of most advanced equipment and state-of-the-art metrology for manufacturing and quality control

Information provided by SCHOTT.

Vendors:
Available Properties
  • Density
  • Hardness, Knoop
  • Hardness, Mohs
  • Tensile Strength at Break
  • Modulus of Elasticity
  • Flexural Strength
  • Flexural Modulus
  • Compressive Modulus
  • Bulk Modulus
  • Poissons Ratio
  • Shear Modulus
  • Volume Resistivity
  • Volume Resistivity
  • Volume Resistivity
  • Dielectric Constant, E perpendicular to c-axis
  • Dielectric Constant, E parallel to c-axis
  • Dielectric Strength
  • Dissipation Factor
  • CTE, linear
  • Specific Heat Capacity
  • Thermal Conductivity
  • Melting Point
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Schott Glas Mainz

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.