MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Covestro Makrolon® SF805 Polycarbonate, 5% Glass Filled
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, 10% Glass Filled

Material Notes: MVR (300 °C/1.2 kg) 7.0 cm³/10 min; structural foam; 5 % glass fiber reinforced; flame retardant; high viscosity; easy release; injection molding; available in natural (opaque) and opaque colors; in combination with an appropriate blowing agent for the production of structural foam moldings

As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.

Vendors:
Available Properties
  • Bulk Density, ISO 60, pellets
  • Density, ISO 1183
  • Moisture Absorption at Equilibrium, ISO 62
  • Water Absorption at Saturation, ISO 62
  • Linear Mold Shrinkage, Flow, ISO 294-4, 60x60x2 mm; 500 bar
  • Linear Mold Shrinkage, Transverse, ISO 294-4, 60x60x2 mm; 500 bar
  • Melt Flow, ISO 1133
  • Puncture Resistance, ISO 6603-2
  • Puncture Resistance, ISO 6603-2
  • Ball Indentation Hardness, b.o. ISO 2039-1, Foamed 6.0 mm; density in the foamed state 900-1000 kg/m3
  • Ball Indentation Hardness, ISO 2039-1
  • Tensile Strength at Break, b.o. ISO 527-1,-2, 5 mm/min; Foamed 6.0 mm; density in the foamed state 900-1000 kg/m3
  • Tensile Strength at Break, ISO 527-1/-2, 5 mm/min
  • Tensile Strength, Yield, ISO 527-1/-2, 5 mm/min
  • Elongation at Break, b.o. ISO 527-1,-2, 5 mm/min; Foamed 6.0 mm; density in the foamed state 900-1000 kg/m3
  • Elongation at Break, ISO 527-1/-2, 5 mm/min
  • Elongation at Yield, ISO 527-1/-2, 5 mm/min
  • Elongation at Yield, ISO 178, 2 mm/min
  • Tensile Modulus, b.o. ISO 527-1,-2, 1 mm/min; Foamed 6.0 mm; density in the foamed state 900-1000 kg/m3
  • Tensile Modulus, ISO 527-1/-2, 1 mm/min
  • Flexural Strength, b.o. ISO 178, 2 mm/min; Foamed 6.0 mm; density in the foamed state 900-1000 kg/
  • Flexural Strength, ISO 178, Flexural strain, 2 mm/min
  • Flexural Yield Strength, b.o. ISO 178, 2 mm/min; Foamed 6.0 mm; density in the foamed state 900-1000 kg/
  • Flexural Yield Strength, ISO 178, 2 mm/min
  • Flexural Modulus, b.o. ISO 178, 2 mm/min; Foamed 6.0 mm; density in the foamed state 900-1000 kg/
  • Flexural Modulus, ISO 178, 2 mm/min
  • Flexural Strain at Yield, b.o. ISO 178, 2 mm/min; Foamed 6.0 mm; density in the foamed state 900-1000 kg/m3
  • Izod Impact, Notched (ISO), ISO 7391/b.o. ISO 180-A, complete break
  • Charpy Impact Unnotched, b.o. ISO 179-1eU, Foamed 6.0 mm; density in the foamed state 900-1000 kg/m3
  • Charpy Impact Unnotched, b.o. ISO 179-1eU, Foamed 6.0 mm; density in the foamed state 900-1000 kg/m3
  • Charpy Impact Unnotched, ISO 179-1eU, complete break
  • Charpy Impact Unnotched, ISO 179-1eU, complete break
  • Charpy Impact Unnotched, ISO 179-1eU, complete break
  • Charpy Impact Unnotched, ISO 179-1eU, complete break
  • Charpy Impact, Notched, ISO 7391/b.o. ISO 179-1eA, complete break
  • Puncture Energy, ISO 6603-2
  • Puncture Energy, ISO 6603-2
  • Volume Resistivity, IEC 60093
  • Surface Resistance, IEC 60093
  • Dielectric Constant, IEC 60250
  • Dielectric Constant, IEC 60250
  • Dielectric Strength, IEC 60243-1, 1 mm
  • Dissipation Factor, IEC 60250
  • Dissipation Factor, IEC 60250
  • Comparative Tracking Index, ISO 60112, CTI M; Solution B
  • Comparative Tracking Index, IEC 60112, Solution A
  • CTE, linear, Parallel to Flow, ISO 11359-1/-2
  • CTE, linear, Transverse to Flow, ISO 11359-1/-2
  • Thermal Conductivity, ISO 8302, cross-flow
  • Hot Ball Pressure Test, IEC 60695-10-2
  • Deflection Temperature at 0.46 MPa (66 psi), b.o. ISO 75-1,-2, Foamed 6.0 mm; density in the foamed state 900-1000 kg/m3
  • Deflection Temperature at 0.46 MPa (66 psi), ISO 75-1/-2
  • Deflection Temperature at 1.8 MPa (264 psi), b.o. ISO 75-1,-2, Foamed 6.0 mm; density in the foamed state 900-1000 kg/m3
  • Deflection Temperature at 1.8 MPa (264 psi), ISO 75-1/-2
  • Vicat Softening Point, ISO 306, 50°C/h 50N
  • Vicat Softening Point, Foamed 6.0 mm; density in the foamed state 900-1000 kg/m3
  • UL RTI, Electrical, UL 746B
  • UL RTI, Mechanical with Impact, UL 746B
  • UL RTI, Mechanical without Impact, UL 746B
  • Flammability, UL94, IEC 60695-11-10
  • Flammability, UL94, o. ISO 306, Foamed 6.0 mm; density in the foamed state 900-1000 kg/m3
  • Flammability, UL94, Foamed 6.0 mm; density in the foamed state 900-1000 kg/m3
  • Flammability, UL94
  • Oxygen Index, ISO 4589-1/-2, Method A
  • Glow Wire Ignition Temperature, IEC 60695-2-13
  • Glow Wire Ignition Temperature, IEC 60695-2-13
  • Glow Wire Ignition Temperature, IEC 60695-2-13
  • Glow Wire Flammability Index, IEC 60695-2-12
  • Glow Wire Flammability Index, IEC 60695-2-12
  • Glow Wire Flammability Index, IEC 60695-2-12
  • Glow Wire Flammability Index, IEC 60695-2-12
  • Melt Temperature, ISO 294, Injection Molding
  • Mold Temperature, ISO 294, Injection Molding
  • Injection Velocity, ISO 294
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Covestro Deutschland AG, Bayer MaterialScience

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.