MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Tropical Obeche Wood
Categories: Wood and Natural Products; Wood; Hardwood

Material Notes: Data is based on small, clear, air-dried samples unless specified.
Usual surface texture: Medium
Dimensional changes when dried lumber is subjected to variations in humidity during service: Small
Resistance to fungal decay (Heartwood in ground contact): Non-durable (5 to 10 years)
Resistance to penetration by preservatives: Resistant
Common Applications: Interior joinery, furniture. Plywood

Key Words: Triplochiton Scleroxylon; Lumber, Timber
Vendors:
Available Properties
  • Specific Gravity, Green, African Origin
  • Density, Air Dry (12-15% Moisture Content)
  • Hardness, Wood Indentation, Side Hardness, Green, African Origin
  • Hardness, Wood Indentation, Side Hardness, 12% Moisture, African Origin
  • Hardness, Wood Indentation, Side
  • Tensile Strength, Ultimate, Perpendicular to Grain
  • Tensile Strength, Ultimate, Axial
  • Modulus of Rupture, Static Bending, Green, African Origin
  • Modulus of Rupture, Static Bending, 12% Moisture, African Origin
  • Modulus of Rupture, Static Bending
  • Flexural Modulus, Static Bending, Green, African Origin
  • Flexural Modulus, Static Bending, 12% Moisture, African Origin
  • Flexural Modulus, Static Bending
  • Compressive Strength, Parallel to Grain, Green, African Origin
  • Compressive Strength, Parallel to Grain, 12% Moisture, African Origin
  • Compressive Strength
  • Machinability, Good Relative to Other Wood
  • Shear Strength, Parallel to Grain, Green, African Origin
  • Shear Strength, Orientation Unknown
  • Shear Strength, Parallel to Grain, 12% Moisture, African Origin
  • Work to Maximum Load, Static Bending, Green, African Origin
  • Work to Maximum Load, Static Bending, 12% Moisture, African Origin
  • Toughness, 2 cm x 2 cm sample
  • Shrinkage, Axial; Green to Zero Moisture
  • Shrinkage, Radial Shrinkage Green to Oven Dry, African Origin
  • Shrinkage, Radial; Green to Zero Moisture
  • Shrinkage, Tangential Shrinkage Green to Oven Dry, African Origin
  • Shrinkage, Tangential; Green to Zero Moisture
  • Shrinkage, Volumetric; Green to Zero Moisture
  • Shrinkage, Volumetric Shrinkage Green to Oven Dry, African Origin
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.