MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Crucible Steel CPM® S110V® Stainless Tool Steel
Categories: Metal; Ferrous Metal; Martensitic; Stainless Steel; Tool Steel

Material Notes: CPM S110V is a high alloy martensitic stainless tool steel produced by the Crucible Particle Metallurgy (CPM) process. CPM S110V contains a high volume fraction of both vanadium-rich and niobium-rich primary alloy carbides for exceptionally good wear resistance compared to other commercially available PM tool steels. It also offers better corrosion resistance than 440C or CPM S90V.

CPM S110V is available on special request in the as-HIP condition or as a clad layer on components. It is not available in forged or rolled bar lengths.

The CPM process results in a fine and uniform carbide distribution in CPM S110V compared to conventionally produced high alloy tool steels which results in relatively good machining, grinding, and toughness characteristics despite the high alloy content.

Information provided by Crucible Industries

Vendors:
Available Properties
  • Hardness, Rockwell C, austenitized at 2150°F then quenched and tempered
  • Hardness, Rockwell C, austenitized at 2150°F then quenched and tempered
  • Hardness, Rockwell C, austenitized at 2150°F then quenched and tempered
  • Hardness, Rockwell C, austenitized at 2150°F then quenched and tempered
  • Hardness, Rockwell C, austenitized at 2150°F then quenched and tempered
  • Hardness, Rockwell C, austenitized at 2150°F then quenched and tempered
  • Hardness, Rockwell C, austenitized at 2150°F then quenched and tempered
  • Hardness, Rockwell C, austenitized at 2150°F then quenched and tempered
  • Carbon, C
  • Chromium, Cr
  • Cobalt, Co
  • Iron, Fe, as balance
  • Molybdenum, Mo
  • Niobium, Nb (Columbium, Cb)
  • Vanadium, V
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.