MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Eastman Abalyn™ D-E Methyl Ester of Rosin
Categories: Fluid

Material Notes: Product Description: Abalyn™ D-E Methyl Ester of Rosin, is an amber-colored, near-neutral, tacky, viscous liquid. It is resinous in nature with clarity and high refractive index, low vapor pressure, high boiling point, and good thermal stability. It has excellent surface-wetting properties. These physical properties, plus its wide compatibility, make it useful in a variety of applications, including lacquers, inks, paper coatings, varnishes, adhesives, sealing compounds, plastics and wood preservatives. To assure minimum odor of products in which it is used, it is given a special steam sparging treatment.

Applications/Uses:

  • Asphalt Modification
  • Assembly
  • Contact Adhesives
  • Hot Melt Adhesives
  • Laminating
  • Packaging
  • Pressure sensitive adhesives
  • Solventborne Adhesives
  • Tapes and Labels
  • Waterborne Adhesives
  • Wax Modification
Key Attributes:
  • Alcohol-soluble
  • Excellent perfume fixative
  • Excellent surface wetting and adhesion properties
  • Excellent wood preservative
  • Insoluble in water
  • Liquid tackifier and plasticizer resin for a wide variety of raw materials and polymers

Information provided by Eastman

Vendors:
Available Properties
  • Density
  • Brookfield Viscosity, LVTD, spindle 31
  • Total Acid Number, mg KOH/g
  • Flash Point
  • Refractive Index
  • Gardner Color Number
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Eastman Chemical Company

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.