MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Rogers Corporation RT/duroid® 6006 Ceramic-PTFE Composite Microwave Laminate
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE); Polytetrafluoroethylene (PTFE), Glass Filled, Molded

Material Notes: Features:
  • High dielectric constant for circuit size reduction
  • Low loss - Ideal for operating at X-band or below
  • Tight dielectric constant and thickness control for repeatable circuit performance
  • Low moisture absorption. Reduces effects of moisture on electrical loss
  • Cladding - EDC or rolled copper foil, also thick aluminum, brass or copper plate (one side)
  • Lead-free process compatible

Typical Applications:

  • Space Saving Circuitry
  • Patch Antennas
  • Ground Radar Warning Systems
  • Satellite Communications Systems
  • Power Amplifiers
  • Aircraft Collision Avoidance Systems

Information provided by Rogers Corporation.

Vendors:
Available Properties
  • Density, ASTM D792
  • Moisture Absorption at Equilibrium, IPC-TM-650 2.6.2.1, 0.05 in.
  • Thickness, Range of Standard Thicknesses
  • Deformation, ASTM D621, Z direction; 24 hrs
  • Deformation, ASTM D621, Z direction; 24 hrs
  • Tensile Strength, Ultimate, ASTM D638, Y direction; 0.1/min strain rate
  • Tensile Strength, Ultimate, ASTM D638, X direction; 0.1/min strain rate
  • Elongation at Break, ASTM D638, Y direction; 0.1/min strain rate
  • Elongation at Break, ASTM D638, X direction; 0.1/min strain rate
  • Tensile Modulus, ASTM D638, Y direction; 0.1/min strain rate
  • Tensile Modulus, ASTM D638, X direction; 0.1/min strain rate
  • Flexural Strength, ASTM D790, Condition A
  • Flexural Modulus, ASTM D790, Y direction, Condition A
  • Flexural Modulus, ASTM D790, X direction, Condition A
  • Compressive Yield Strength, ASTM D695, Z direction; 0.05/min strain rate
  • Compressive Modulus, ASTM D695, Z direction; 0.05/min strain rate
  • Peel Strength, IPC-TM-650 2.4.8, Copper, after solder float
  • Volume Resistivity, IPC 2.5.17.1, Condition A
  • Surface Resistance, IPC 2.5.17.1, Condition A
  • Dielectric Constant, IPC-TM-650 2.5.5.5, Process, Clamped stripline, Z-direction
  • Dielectric Constant, Differential Phase Length Method, Design, Z-direction
  • Dissipation Factor, IPC-TM-650 2.5.5.5, Z direction
  • CTE, linear, ASTM D3386, Y-Direction; 5°C/min
  • CTE, linear, ASTM D3386, X-Direction; 5°C/min
  • CTE, linear, ASTM D3386, Z-Direction; 5°C/min
  • Specific Heat Capacity, calculated
  • Thermal Conductivity, ASTM C518
  • Decomposition Temperature, ASTM D3850, TGA
  • Flammability, UL94
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.