MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Cosmic Plastics K31/6220 Short Glass Fiber Filled Diallyl Iso-Phthalate Molding Compound
Categories: Polymer; Thermoset; Diallyl Phthalate (DAP); Diallyl Phthalate (DAP) Molding Compound, Short Glass Fiber Filled

Material Notes: Description: Cosmic K31 / 6220 is a short glass fiber filled, high heat resistant general purpose diallyl iso-phthalate molding compound which is supplied in a granular form. It pours easily, can be preformed, and molds easily in standard compression , transfer or injection equipment. K31 has FDA approval for direct food contact use.

Features: K31 / 6220 has good impact strength, excellent electrical properties and very high heat service properties.

Applications: The high strength of this material makes it ideal for switches, terminals, housings, structural parts and insulators.

Information provided by Cosmic Plastics Inc

Vendors:
Available Properties
  • Specific Gravity
  • Bulk Factor
  • Water Absorption
  • Linear Mold Shrinkage
  • Tensile Strength at Break
  • Flexural Strength
  • Compressive Strength
  • Izod Impact, Notched
  • Volume Resistivity
  • Volume Resistivity, 100% RH
  • Surface Resistance
  • Surface Resistance, 100% RH
  • Dielectric Constant, Dry
  • Dielectric Constant, Dry
  • Dielectric Constant, Wet
  • Dielectric Constant, Wet
  • Dielectric Strength, Dry, step by step
  • Dielectric Strength, Wet, step by step
  • Dielectric Breakdown, Wet, step by step
  • Dielectric Breakdown, Dry, step by step
  • Dissipation Factor, Dry
  • Dissipation Factor, Wet
  • Dissipation Factor, Dry
  • Dissipation Factor, Wet
  • Arc Resistance
  • CTE, linear
  • Heat Distortion Temperature
  • Mold Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.