Description: Apcoflex® N745 is a cold polymerized, medium ACN containing acrylonitrile butadiene co-polymer. It contains non-staining antioxidant. Applications: Apcoflex® N745 is a medium viscosity highly suitable for the manufacture of products where excellent thermal, abrasion and fuel resistances are desired. It is specifically designed for applications where easy processibility and filler incorporation with low heat build-up is required and is thus recommended for variety of extruded and moulded rubber goods such as Cable covers, hoses, Rice and Industrial rollers etc. CAS No,: 9003-18-3 Information provided by Apcotex Industries Limited |