Balance of stiffness and toughness, High impact, USP Class VI Applications: Razor components, Personal care, Consumer goods In addition, exposure to gamma radiation in the 2.02-6.06 megarad range ahs no significant effect on the physical and optical properties of the material. Properties were determined on injection molded specimens at 23°C and 50% R.H. unless otherwise specified. Information provided by NOVA Chemicals. This grade no longer in product line. INEOS NOVA began October 1 2007 as an expansion of the 50:50 joint venture between NOVA Chemicals and INEOS to include North American assets. |