MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Alpase M-5™ Aluminum Mold Plate
Categories: Metal; Nonferrous Metal; Aluminum Alloy; Aluminum Casting Alloy

Material Notes:
  • Excellent weldability
  • Surface Condition - Machined top and bottom to reduce costly handling and machining steps
  • Dimensional Stability - High dimensional stability during and after machining
  • Polishing - Good polishing properties
  • Good Anodizing and Hard Coating properties
  • Corrosion Resistance - Excellent corrosion resistance in many applications
  • Low density offers a 5% weight savings over other cast products
  • Very consistent hardness and mechanical properties throughout its entire thickness range, regardless of size.
  • Vacuum tight microstructure

Applications: Injection Molds, Blow Molds, Structural Foam Molds, and Rubber Molds. Additional uses include: Vacuum Forming Tools, Compression Molds, Heating and Cooling Plates and proven Semi-conductor Transfer Chamber applications.

Sizes: Thickness up to 30 inches; Width up to 88 inches; Length up to 195 inches.

Typical data provided by Alpase.

Key Words: Aluminium; U/T inspected to MIL-Spec 2154 Class A
Vendors:
Available Properties
  • Density
  • Density
  • Hardness, Brinell
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Modulus of Elasticity
  • Modulus of Elasticity
  • Electrical Resistivity
  • CTE, linear
  • CTE, linear
  • Thermal Conductivity
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.