MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Evonik TEGOMER® DA 640 Dispersant
Categories: Other Engineering Material

Material Notes: Product description: TEGOMER® DA 640 is an anionic modified polyether to be used for the following main application:
  • dispersing of fillers as well as of inorganic and organic pigments in water-based systems
  • flocculation of inorganic pigments or fillers
  • emulsifier for the polymerization
Application: TEGOMER® DA 640 is a liquid dispersing additive used for surface wetting to improve dispersion properties of:
  • inorganic fillers e. g. talc, barium sulfate
  • inorganic pigments e. g. titanium dioxide, Ultramarine blue, iron oxides
  • organic pigments and carbon blacks can be dispersed as well with higher addition levels
TEGOMER® DA 640 is suitable at lower addition levels to be used as flocculent for inorganic particles only, e. g. titanium dioxide, metal hydroxides TEGOMER® DA 640 is a primary or secondary emulsifier for the polymerization of acrylates or PVAc.

Benefits: The use of TEGOMER® DA 640 offers several advantages in dependence on the function used:

  • higher filling of pastes at low addition levels in combination with excellent rheological properties and no occurrence of gelling
  • higher color strength respectively improved hiding power for titanium dioxide pastes
  • improved water repellency which goes parallel with the flocculation ability of high density materials
  • improved durability due to hydrophobic character when used for surface treatment
  • less abrasion of doctor blades using filler or titanium dioxide pastes for the application of paper coatings
  • water-based formulations which contain significant amounts of glycol or other solvents can be stabilized as well
  • solvent- and nonylphenol ethoxylate-free emulsifier technology
  • pure acrylates as well as those with high EHA content for adhesive formulation reach fine particle size distribution if it is used as emulsifier
  • water pick up of emulsions and pigments/ fillers is lowered

Information provided by Evonik

Vendors:
Available Properties
  • pH
  • Viscosity
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Evonik Corporation (Former Evonik Degussa GmbH)

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.