MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
NRI Acid Coat Flexible, Chemical Resistant, Urethane Polymer Coating
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: Description: Acid-Coat™ is a high performance, chemically resistant coating specifically designed for applications where high concentrations of acids and alkali are present. It provides excellent resistance to nitric acid, hydrochloric acid, phosphoric acid, sodium hydroxide, sulfuric acid, Clorox and ammonia. When fully cured Acid-Coat provides excellent abrasion, impact and corrosion resistance to metal, wood, fiberglass and masonry surfaces. It offers easy mixing and simple application by brush or paint roller. Acid-Coat can be mixed with sand and or aluminum oxide grit additives to provide an aggressive non-skid surface in both wet and dry environments. The kit is packaged in one gallon containers complete with 1 quart activator and your choice of 17 color options. Acid-Coat provides a tough, high build, protective coating that can be applied in wet film thickness up to 1/8” without sagging, with low VOC’s, good UV and excellent chemical resistance.

Typical Applications:

  • Pipe, tank, or surface coating
  • Application to metals, wood, & concrete
  • Abrasion resistance coating
  • Waterproofing
  • Non-slip surfacing
Benefits:
  • Excellent chemical resistance to chlorines and acids
  • Waterproof, UV, and chemically resistant coating
  • Easy application
  • Packaged in convenient one gallon kits
  • UV Stable (color pigment, non-white

Information provided by NRI® Innovative Composite Solutions

Vendors:
Available Properties
  • Volatile Organic Compounds (VOC) Content, 66% solid
  • Hardness, Shore A, ASTM D2240-85
  • Tensile Strength, ASTM D412
  • Elongation at Break, ASTM D412
  • Tear Strength, ASTM D624
  • Abrasion, ASTM D3389-94, [mg] abrasion loss per 1k revolutions
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Cure Time, 75% cure
  • Cure Time, 95% cure
  • Pot Life
  • Shelf Life
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.