MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Extreme Materials from MCAM
Visit Mitsubishi Chemical Advanced Materials for Extreme Materials - high performance plastic machining stock engineered to replace metals such as nickel alloys or stainless steel.
Overview of materials for Nickel Alloy
Categories: Metal; Nonferrous Metal; Nickel Alloy

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Nickel Alloy". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors:
Available Properties
  • Density, Average value: 8.39 g/cc Grade Count:947
  • Porosity, Average value: 3.06 % Grade Count:10
  • Particle Size, Average value: 41.2 µm Grade Count:71
  • Thickness, Average value: 2490 microns Grade Count:8
  • Hardness, Brinell, Average value: 282 Grade Count:117
  • Hardness, Knoop, Average value: 329 Grade Count:90
  • Hardness, Rockwell A, Average value: 60.8 Grade Count:46
  • Hardness, Rockwell B, Average value: 88.1 Grade Count:149
  • Hardness, Rockwell C, Average value: 38.0 Grade Count:227
  • Hardness, Vickers, Average value: 295 Grade Count:189
  • Tensile Strength, Ultimate, Average value: 903 MPa Grade Count:885
  • Tensile Strength, Yield, Average value: 597 MPa Grade Count:786
  • Elongation at Break, Average value: 33.7 % Grade Count:811
  • Reduction of Area, Average value: 45.8 % Grade Count:181
  • Modulus of Elasticity, Average value: 207 GPa Grade Count:568
  • Flexural Yield Strength, Average value: 481 MPa Grade Count:21
  • Flexural Modulus, Average value: 76.4 GPa Grade Count:7
  • Compressive Yield Strength, Average value: 783 MPa Grade Count:12
  • Poissons Ratio, Average value: 0.328 Grade Count:155
  • Fatigue Strength, Average value: 508 MPa Grade Count:18
  • Shear Modulus, Average value: 77.5 GPa Grade Count:127
  • Shear Strength, Average value: 723 MPa Grade Count:6
  • Adhesive Bond Strength, Average value: 483 MPa Grade Count:3
  • Izod Impact, Average value: 131 J Grade Count:6
  • Izod Impact, Unnotched, Average value: 0.966 J/cm Grade Count:5
  • Charpy Impact, Average value: 151 J Grade Count:125
  • Charpy Impact, Unnotched, Average value: 26.7 J Grade Count:8
  • Charpy Impact Unnotched, Average value: 9.57 J/cm² Grade Count:5
  • Coefficient of Friction, Average value: 0.188 Grade Count:5
  • Tensile Set, Average value: 0.260 % Grade Count:5
  • Electrical Resistivity, Average value: 0.000104 ohm-cm Grade Count:665
  • Surface Resistance, Average value: 0.127 ohm Grade Count:3
  • Magnetic Permeability, Average value: 21000 Grade Count:162
  • Magnetic Coercive Force, Hc, Average value: 662 Oe Grade Count:22
  • Magnetic Saturation Flux Density, Bmax, Average value: 9550 Gauss Grade Count:8
  • Magnetic Remanence, Br, Average value: 8120 Gauss Grade Count:17
  • Magnetic Maximum Energy Product, BH, Average value: 3.99 MGOe Grade Count:12
  • Magnetic Susceptibility, Average value: 4.31 Grade Count:5
  • Curie Temperature, Average value: 233 °C Grade Count:131
  • Shielding Effectiveness, Average value: 80.0 dB Grade Count:6
  • CTE, linear, Average value: 14.1 µm/m-°C Grade Count:664
  • Specific Heat Capacity, Average value: 0.431 J/g-°C Grade Count:440
  • Thermal Conductivity, Average value: 16.7 W/m-K Grade Count:530
  • Melting Point, Average value: 1320 °C Grade Count:747
  • Solidus, Average value: 1290 °C Grade Count:559
  • Liquidus, Average value: 1360 °C Grade Count:559
  • Maximum Service Temperature, Air, Average value: 810 °C Grade Count:193
  • Minimum Service Temperature, Air, Average value: -22.3 °C Grade Count:8
  • Emissivity (0-1), Average value: 0.880 Grade Count:14
  • Processing Temperature, Average value: 579 °C Grade Count:8
  • Annealing Temperature, Average value: 1110 °C Grade Count:51
  • Aging Temperature, Average value: 713 °C Grade Count:12
  • Hot-Working Temperature, Average value: 1050 °C Grade Count:13
  • Casting Temperature, Average value: 1330 °C Grade Count:6
  • Al + Ti, Average value: 0.675 % Grade Count:12
  • Aluminum, Al, Average value: 1.81 % Grade Count:532
  • Beryllium, Be, Average value: 2.22 % Grade Count:26
  • Bismuth, Bi, Average value: 0.000344 % Grade Count:3
  • Boron, B, Average value: 0.651 % Grade Count:374
  • Carbon, C, Average value: 0.167 % Grade Count:960
  • Cb + Ta, Average value: 3.93 % Grade Count:5
  • Chromium, Cr, Average value: 17.9 % Grade Count:933
  • Cobalt, Co, Average value: 6.13 % Grade Count:582
  • Copper, Cu, Average value: 4.72 % Grade Count:355
  • Hafnium, Hf, Average value: 0.833 % Grade Count:3
  • Hydrogen, H, Average value: 0.00433 % Grade Count:6
  • Iron, Fe, Average value: 7.76 % Grade Count:997
  • Lanthanum, La, Average value: 0.481 % Grade Count:73
  • Lead, Pb, Average value: 0.0128 % Grade Count:6
  • Magnesium, Mg, Average value: 0.0381 % Grade Count:15
  • Manganese, Mn, Average value: 0.843 % Grade Count:776
  • Molybdenum, Mo, Average value: 10.3 % Grade Count:654
  • Nb + Ta, Average value: 1.47 % Grade Count:32
  • Nickel, Ni, Average value: 64.3 % Grade Count:1191
  • Niobium, Nb (Columbium, Cb), Average value: 3.09 % Grade Count:208
  • Nitrogen, N, Average value: 0.0187 % Grade Count:23
  • Oxygen, O, Average value: 0.0317 % Grade Count:16
  • Phosphorus, P, Average value: 0.207 % Grade Count:280
  • Rhenium, Re, Average value: 2.07 % Grade Count:3
  • Selenium, Se, Average value: 0.00423 % Grade Count:10
  • Silicon, Si, Average value: 0.966 % Grade Count:878
  • Silver, Ag, Average value: 16.5 % Grade Count:4
  • Sulfur, S, Average value: 0.0165 % Grade Count:407
  • Tantalum, Ta, Average value: 2.10 % Grade Count:24
  • Tin, Sn, Average value: 0.216 % Grade Count:4
  • Titanium, Ti, Average value: 2.40 % Grade Count:417
  • Tungsten, W, Average value: 4.96 % Grade Count:305
  • Vanadium, V, Average value: 0.482 % Grade Count:98
  • WC, Average value: 55.0 % Grade Count:4
  • Y2O3, Average value: 0.600 % Grade Count:4
  • Yttrium, Y, Average value: 0.134 % Grade Count:44
  • Zinc, Zn, Average value: 0.251 % Grade Count:6
  • Zirconium, Zr, Average value: 0.501 % Grade Count:82
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.