A homopolymer resin designed for spun bond non-wovens. the resin is particularly suited for excellent spinning for uniform, high quality fabrics. Formulated for applications requiring low color and low gas fading discoloration. produced with a catalyst system that does not include intentionally added phthalate compounds. PP3155E5 is the version of PP3155 and / or PP3155E3 based on catalyst system which does not include intentionally added phthalates and contains a non-gas fade additive package. Availability: Asia Pacific, North America. Features: good processability, non intentionally added phthalates. Applications: Fibers, medical/healthcare, spun bond non-wovens, industrial applications, personal care. Appearance: natural color. Forms: pellets. Processing Method: filament extrusion, spun bond non-wovens. Information provided by ExxonMobil. |