MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
CRP  Windform
Mitsubishi PC 3D Printing Filament
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: PC is a high-performance plastic that possesses a unique balance of toughness, dimensional stability, optical clarity, high heat resistance and excellent electrical resistance. PC is commonly used to make all sorts of products including bullet-proof glass, riot shields, cell phone exteriors and many other products that require an engineering grade material. We recommend PC for more experienced users that are looking to extend their filament options.

Features:

  • Great strength & stiffness
  • High optical clarity
  • Resistant to high temperatures up to 140°C
  • Low flammability (UL-94 V2)
Colors: PC is available from stock in 1 clear color. Other colors on request

Information provided by Mitsubishi Chemical.

Vendors:
Available Properties
  • Specific Gravity, ISO 1183
  • Filament Diameter, Tolerance: 50 µm, =95% Roundness
  • Filament Diameter, Tolerance: 100 µm, =95% Roundness
  • Melt Flow, ISO 1133
  • Storage Temperature
  • Tensile Strength at Break, ISO 527
  • Tensile Strength, Yield, ISO 527
  • Elongation at Break, ISO 527
  • Tensile Modulus, ISO 527, (E)
  • Charpy Impact, Notched, ISO 179 1eA
  • Deflection Temperature at 1.8 MPa (264 psi), ISO 75
  • Vicat Softening Point, ISO 306 B50
  • Processing Temperature, Printing Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.