MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Excel Industries EXFLAR™ N Flame Retardants
Categories: Other Engineering Material

Material Notes: Advantage:
  • Thermally stable up to 320oC, it finds applications in polymers processed at elevated temperatures.
  • Naturally suited for PA_6 and PA_66 both in unfilled (UL 94 V_0) and filled (UL 94 V_2) grades.
  • Effective in polyesters, epoxy resins, polyolefins when used with appropriate synergists.
  • Environmentally friendly with its non toxic, non corrosive nature and halogen free composition.
  • Nitrogen based, Intumescent Flame Retardant
  • Coarse Powder suitable for compounding applications
  • Non Toxic, Non Corrosive, Stable upto 320oC
  • Suitable for wide range of polymers
  • Enables eco label compliance in end use

Information provided by Excel Industries Ltd.

Vendors:
Available Properties
  • Bulk Density
  • Particle Size, 100% passing
  • pH, 5% aqueous solution
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.