MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Overview of materials for Thermoset Fluoroelastomer
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Fluoroelastomer". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors:
Available Properties
  • Density, Average value: 1.87 g/cc Grade Count:612
  • Oxygen Transmission, Average value: 105 cc-mm/m²-24hr-atm Grade Count:40
  • Viscosity, Average value: 89.8 cP Grade Count:7
  • Viscosity, Average value: 56.8 cP Grade Count:14
  • Mooney Viscosity, Average value: 55.2 Grade Count:490
  • Molecular Weight, Average value: 3000 g/mol Grade Count:3
  • Evaporation Loss, Average value: 2.00 % Grade Count:3
  • Evaporation Loss, Average value: 2.00 % Grade Count:3
  • Hardness, Shore A, Average value: 73.6 Grade Count:971
  • Hardness, Shore A, Average value: 71.4 Grade Count:1
  • Hardness, Shore A, Average value: 71.4 Grade Count:37
  • Hardness, Shore A, Average value: 71.4 Grade Count:37
  • Hardness, Shore D, Average value: 59.8 Grade Count:4
  • Hardness, Shore M, Average value: 80.0 Grade Count:4
  • Tensile Strength, Ultimate, Average value: 14.6 MPa Grade Count:919
  • Tensile Strength, Ultimate, Average value: 13.4 MPa Grade Count:1
  • Tensile Strength, Ultimate, Average value: 13.4 MPa Grade Count:49
  • Tensile Strength, Ultimate, Average value: 13.4 MPa Grade Count:49
  • Tensile Strength, Yield, Average value: 9.37 MPa Grade Count:225
  • Elongation at Break, Average value: 224 % Grade Count:1055
  • Elongation at Break, Average value: 204 % Grade Count:1
  • Elongation at Break, Average value: 204 % Grade Count:48
  • Elongation at Break, Average value: 204 % Grade Count:48
  • Modulus of Elasticity, Average value: 0.0207 GPa Grade Count:30
  • Modulus of Elasticity, Average value: 0.000480 GPa Grade Count:2
  • Modulus of Elasticity, Average value: 0.000480 GPa Grade Count:2
  • Flexural Modulus, Average value: 0.0100 GPa Grade Count:3
  • Compressive Modulus, Average value: 0.00534 GPa Grade Count:4
  • Rebound, Average value: 8.86 % Grade Count:11
  • Poissons Ratio, Average value: 0.494 Grade Count:19
  • Shear Modulus, Average value: 0.00760 GPa Grade Count:19
  • Shear Modulus, Average value: 0.0430 GPa Grade Count:2
  • Secant Modulus, Average value: 0.0215 GPa Grade Count:19
  • Coefficient of Friction, Average value: 0.791 Grade Count:51
  • Tear Strength Test, Average value: 232 Grade Count:21
  • Tear Strength, Average value: 29.8 kN/m Grade Count:129
  • Tear Strength, Average value: 8.16 kN/m Grade Count:5
  • Compression Set, Average value: 22.7 % Grade Count:1026
  • Electrical Resistivity, Average value: 3.02e+16 ohm-cm Grade Count:51
  • Surface Resistance, Average value: 2.07e+11 ohm Grade Count:3
  • Shielding Effectiveness, Average value: 98.3 dB Grade Count:3
  • Dielectric Constant, Average value: 9.75 Grade Count:44
  • Dielectric Strength, Average value: 23.3 kV/mm Grade Count:46
  • Dissipation Factor, Average value: 0.0292 Grade Count:6
  • CTE, linear, Average value: 263 µm/m-°C Grade Count:71
  • Specific Heat Capacity, Average value: 1.65 J/g-°C Grade Count:40
  • Specific Heat Capacity, Average value: 1.12 J/g-°C Grade Count:6
  • Thermal Conductivity, Average value: 0.235 W/m-K Grade Count:40
  • Thermal Conductivity, Average value: 0.180 W/m-K Grade Count:3
  • Maximum Service Temperature, Air, Average value: 236 °C Grade Count:393
  • Minimum Service Temperature, Air, Average value: -18.6 °C Grade Count:531
  • Brittleness Temperature, Average value: -24.5 °C Grade Count:159
  • Glass Transition Temp, Tg, Average value: -18.7 °C Grade Count:180
  • Transformation Temperature, Average value: -8.54 °C Grade Count:13
  • Flash Point, Average value: 323 °C Grade Count:93
  • Refractive Index, Average value: 1.37 Grade Count:3
  • Transmission, Visible, Average value: 35.8 % Grade Count:6
  • Processing Temperature, Average value: 203 °C Grade Count:151
  • Moisture Content, Average value: 0.500 % Grade Count:7
  • Cure Time, Average value: 32.1 min Grade Count:78
  • Cure Time, Average value: 460 min Grade Count:104
  • Carbon, C, Average value: 21.6 % Grade Count:10
  • Fluorine, F, Average value: 66.8 % Grade Count:340
  • Oxygen, O, Average value: 9.40 % Grade Count:10
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.