MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Evonik tert.-Butanol azetropic Liquid
Categories: Fluid

Material Notes: CAS No: 75-65-0

Properties: Tert.-Butanol is a colorless liquid which solidifies at room temperature. TBA is miscible with nearly all organic solvents (alcohol, ethers, ketones, esters and hydrocarbons) and water, too. TBA and water form an azeotropic mixture having a water content of 11.75%. In contrast to pure tert.-Butanol, the azeotrope is liquid even at room temperature. With strong acids, decomposition can take place mainly to give isobutene. Tert.-Butanol is largely stable to oxidizing agents and halogens, it is non-corrosive. Vapors can form explosive mixtures with air. Concentrated vapors have an anaesthetic effect.anaesthetic effect.

Use: Tert.-Butanol is a starting material for the production of tert.-butyl peroxides as polymerization initators. TBA is used as an alkylating agent for aromatics and phenols for the production of tert.-butylaromatics and, for example, tert.-butyl Cresol; for the production of tert.butyl esters as precursors for antioxidants, phenolic resins, pharmaceutical products dn perfumes. Due to its good dissolving properties and also good solubility in polar and non-polar substance, TBA is outstandingly suitable as a solvent and as a solubiliser, for example in waterbased paints, for the dewaxing of oils and as denaturing agent for Ethanol.

Information provided by Evonik

Vendors:
Available Properties
  • Density, relative
  • Viscosity
  • Molecular Weight
  • Vapor Pressure
  • Vapor Pressure
  • Vapor Pressure
  • Vapor Pressure
  • Vapor Pressure
  • Vapor Pressure
  • Total Acid Number, DIN EN ISO 2114, [mg KOH/g]
  • Dielectric Constant
  • Heat of Vaporization, at bp
  • Specific Heat Capacity
  • Melting Point
  • Boiling Point
  • Refractive Index
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Evonik Corporation (Former Evonik Degussa GmbH)

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.