Veloxx LVP is a two-component, 100% solids, two-phase, epoxy used for priming concrete, masonry or wood surfaces, prior to application of the FiberBond™ Strengthening System. Veloxx LVP is a patented, ICBO/ICCES approved (ER #5836) part of the FiberBond™ Strengthening System, a highly engineered product for the external strengthening of concrete and masonry structures. Advantages: - Developed specifically for the FiberBond™ Strengthening System for concrete and masonry structures.
- Fully compatible with Veloxx LR Laminating Resin and Veloxx AP Adhesive Paste.
- Long pot life.
- Easy to mix.
- Excellent adhesion to concrete and masonry materials.
- Solvent free, VOC compliant.
- Minimum substrate and ambient temperature is 40° F.
Typical Uses: Veloxx LVP is applied by brush or roller to penetrate substrate to provide bond and prevent wicking of the laminating resin.Information provided by Milliken® |