MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
KLJ Group KLJ SC XL 500 XLPE
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Description: KLJ SC XL 500 is a Semi Conducting Thermoplastic Bonded Compound for sioplas application having excellent heat deformation resistant characteristics and specially designed for use as a thermoplastic conductor and insulation shield. Further the material has superior thermal stress crack resistance, toughness to avoid sticking of cable layers at the time of curing. It is also easy to process and has low volume resistivity.

Specifications: KLJ-SC meets the requirement of ICEA S-66-524/NEAM WC7, BS 6622, IEC 60502, IEC 60840

Application: Semiconducting KLJ-SC XL 500 has been designed to meet the conductivity and bondability requirements of both conductor and insulation shield for medium voltage cables. Cables manufactured with KLJ-XL SEM 500 conductor and insulation shields are rated for 90°C continuous service and 130°C overload temperature.

Information provided by KLJ Group

Vendors:
Available Properties
  • Specific Gravity, ASTM D1505
  • Melt Flow, ASTM D1238
  • Hardness, Shore D, ASTM D2240
  • Tensile Strength, ASTM D638
  • Tensile Strength
  • Elongation at Break, ASTM D638
  • Volume Resistivity, ASTM D257
  • Volume Resistivity, ASTM D257
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.