MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Teknor Apex HFFR 2005 Polyolefin, Halogen Free
Categories: Polymer; Thermoplastic; Polyolefin; Polyolefin, Wire/Cable Grade

Material Notes: Notes: RoHS Compliant

Features: Flame Retardant; Halogen Free

Uses: Communication Wire Jacketing; Electronic Cable Jacketing; Security Cable Jacketing; Plenum Cable Jacketing

Agency Ratings: IEC Unspecified Rating; ICEA Unspecified Rating; UL QMTT2 .E200337

Processing Method: Extrusion

Forms: Pellets

Additional Information:

Ultimate Elongation Retained, UL 1581, Oven Aged, 7 days, 100°C: 78%

Tensile Strength Retained, UL 1581, Oven Aged, 7 days, 100°C: 113%

Ultimate Elongation Retained, UL 1581, Oven Aged, 7 days, 113°C: 74%

Tensile Strength Retained, UL 1581, Oven Aged, 7 days, 113°C: 108%

Ultimate Elongation Retained, UL 1581, Oven Aged, 7 days, 125°C: 73%

Tensile Strength Retained, UL 1581, Oven Aged, 7 days, 125°C: 116%

Ultimate Elongation Retained, UL 1581, Oven Aged, 7 days, 136°C: 72%

Tensile Strength Retained, UL 1581, Oven Aged, 7 days, 136°C: 109%

Acid Gas, MIL-C-24643: < 5.0 mg

Acidity of Gases, IEC-754-2: < 6.0 pH

Conductivity: < 2.0 µS/cm

Smoke Index, NES-711: < 10.0

Toxicity Index, NES-713: 0.085

Acid Gas, MIL-C-24643: < 5.0 mg

Acidity of Gases, IEC-754-2: < 6.0 pH

Conductivity: < 2.0 µS/cm

Smoke Index, NES-711: < 10.0

Toxicity Index, NES-713: < 1.0

Cone Calorimeter at 50 kW/m2, Peak Heat Release Rate: 154 kW/m2

Cone Calorimeter at 50 kW/m2, Total Heat Released: 157 MJ/m2

Cone Calorimeter at 50 kW/m2, Peak Smoke: 0.8 1/m

Cone Calorimeter at 50 kW/m2, Time to Sustained Ignition: 138 sec

Information Provided by Teknor Apex

Vendors:
Available Properties
  • Specific Gravity, ASTM D792
  • Melt Flow, ASTM D1238
  • Hardness, Shore D, ASTM D2240, 10 seconds
  • Tensile Strength at Break, ASTM D638
  • Elongation at Break, ASTM D638
  • Volume Resistivity, ASTM D257
  • Dielectric Constant, ASTM D150
  • Dissipation Factor, ASTM D150
  • Brittleness Temperature, ASTM D746
  • Oxygen Index, ASTM D2863
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Teknor Apex Company

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.