MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
SEKISUI SPI KYDEX® 410 ABS/PVC
Categories: Polymer; Thermoplastic; ABS Polymer; ABS/PVC Alloy

Material Notes: Proprietary ABS/PVC sheet

KYDEX® 410 is a proprietary ABS/PVC thermoplastic sheet that offers superior thermoformability, rigidity, breakage resistance, chemical resistance and fire retardancy.

KYDEX® 410 is available in a wide range of standard and custom colors, textures, and sheet sizes. It is Underwriters Laboratories, Inc® recognized for UL std 94 V-0, 5V (rating pending).

Applications:

  • Medical Equipment Housings
  • Electrical Equipment Housings
  • Mass Transit Interior Vehicle Components
  • Miscellaneous Applications

Flammability:

  • FAR 25.853a
  • UL94 V-0, 5V @ 1mm
  • Radiant Panel: RP25
  • FMVSS 302

Features:

  • Good for deep or hard to form parts
  • More rigid, parts will deform less when loaded - or can be down-gauged for weight-savings
  • High Notched Izod impact resistance offers resistance to breakage
  • Meets highest standard for chemical resistance for thermoplastic materials
  • Passes UL Std 94 V-0 and 5V in all thicknesses and colors
  • Uniform wall thickness in crisp detail
  • Easy machining and fabricating using conventional methods and equipment
  • Low moisture absorption - no drying needed prior to thermoforming
  • Passes ball pressure test as per UL 60601-1
  • Good low temperature impact resistance

Information provided by Sekisui Polymer Innovations

Vendors:
Available Properties
  • Specific Gravity, ASTM D792
  • Moisture Absorption, ASTM D570, After three months storage, drying may be required
  • Linear Mold Shrinkage
  • Hardness, Rockwell R, ASTM D785
  • Tensile Strength, ASTM D638
  • Flexural Strength, ASTM D790
  • Flexural Modulus, ASTM D790
  • Izod Impact, Notched, ASTM D256
  • Izod Impact, Notched, ASTM D256
  • CTE, linear, Transverse to Flow, ASTM E831
  • Deflection Temperature at 1.8 MPa (264 psi), ASTM D648, Unannealed
  • Deflection Temperature at 1.8 MPa (264 psi), ASTM D648, Annealed at 65.5°C for 8 hrs and cooled slowly
  • Flammability, UL94, UL File E115252; Component Recognition
  • Flammability, UL94, UL Standard 94, Underwriters Laboratories., Inc®, File E115252; Component Recognition
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.