MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Vycom CELTECĀ® Expanded Rigid foam PVC board
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes: Celtec Displayboard is a foamed polyvinyl chloride (PVC) sheet whose combination of features makes it ideal for signage, exhibits, store displays, POP, Kiosks, screen printing and more. The surface is a smooth matte finish that makes it ideal to paint or laminate to secondary substrates. Celtec also has good screw and staple retention which makes it ideal for stage prop design, cabinetry and other wood replacement projects. Sheets are tough, high-strength and lightweight, and can be ordered in a wide range of sizes, thicknesses and colors. Celtec sheets are free of lead, cadmium, barium and zinc. Celtec is recommended for industrial and commercial signage. It readily accepts virtually any form of graphic overlay (print, paint and photo mounting). Celtec is also easy to cut and shape, making it a strong choice for three-dimensional exhibits, displays and stage sets.

FEATURES AND BENEFITS

  • Lightweight- Celtec is easy to handle, easy to work with.
  • Low Flammability- Celtec meets UL94 5V, UL 1975 and has a flame spread of 20 according to ASTM E84.
  • Water resistant- Celtec has a closed cell structure and has extremely low water absorption values.
  • Surface- Celtecs smooth matte surface is ideal for graphics, printing and laminating.
  • Weatherability- Celtec is more color-fast than other foam PVC products.
  • Strength- Celtec has an excellent strength to weight ratio as shown in the screw and staple pull test data.
  • Thermal Conductivity- Celtec has excellent insulating characteristics.
  • Safety- Celtec contains no lead, cadmium or zinc.

Information provided by Compression Polymers Corp - Vycom

Vendors:
Available Properties
  • Density, ASTM D792
  • Density, ASTM D792
  • Water Absorption, ASTM D570
  • Water Absorption, ASTM D570
  • Water Absorption, ASTM D2842
  • Tensile Strength, Ultimate, ASTM D638
  • Tensile Strength, Ultimate, ASTM D638
  • Tensile Modulus, ASTM D638
  • Tensile Modulus, ASTM D638
  • Flexural Strength, ASTM D790
  • Flexural Modulus, ASTM D790
  • Izod Impact, Notched, ASTM D256
  • Charpy Impact, Unnotched, ASTM D256
  • Charpy Impact, Unnotched, ASTM D256
  • Gardner Impact, ASTM D4228
  • Dielectric Strength, ASTM D149
  • CTE, linear, ASTM D696
  • CTE, linear, ASTM D696
  • Thermal Conductivity, ASTM C177
  • Deflection Temperature at 1.8 MPa (264 psi), ASTM D648
  • Deflection Temperature at 1.8 MPa (264 psi), ASTM D648
  • Flammability, UL94, 5V
  • Flame Spread Index, ASTM E84
  • Flame Spread Index, ASTM E84
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
CPC - Vycom Co. Compression Plastics Corporation

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.