MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
3M Dynamar™ RC 3630 Rubber Curative  (discontinued **)
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Product Description: 3M™ Dynamar™ RC 3630 is a pelletized FKM crosslinker that offers easy incorporation with excellent dispersion characteristics. Used in combination with 3M™ Dynamar™ RC 3620, Dynamar RC 3630 affords you the flexibility to customize your compound formulations.

Features and Benefits:

  • FKM crosslinker for adjusting crosslink density
  • Can be used to retard cure
  • Excellent dispersion characteristics
  • 3M technical service available for developing compound formulations

Information provided by 3M™

Vendors:
Available Properties
  • Specific Gravity
  • Hardness, Shore A, ASTM D2240, Low Crosslink, Press Cure 10 Minutes @ 177°C (350°F) Post Cure 16 Hours @ 232°C (450°F)
  • Hardness, Shore A, ASTM D2240, High Crosslink, Press Cure 10 Minutes @ 177°C (350°F) Post Cure 16 Hours @ 232°C (450°F)
  • Hardness, Shore A, ASTM D573, Low Crosslink, Heat Aged
  • Hardness, Shore A, ASTM D573, High Crosslink, Heat Aged
  • Tensile Strength, ASTM D412, Low Crosslink, Press Cure 10 Minutes @ 177°C (350°F) Post Cure 16 Hours @ 232°C (450°F)
  • Tensile Strength, ASTM D412, High Crosslink, Press Cure 10 Minutes @ 177°C (350°F) Post Cure 16 Hours @ 232°C (450°F)
  • Tensile Strength, ASTM D573, Low Crosslink, Heat Aged
  • Tensile Strength, ASTM D573, High Crosslink, Heat Aged
  • Elongation at Break, ASTM D412, High Crosslink, Press Cure 10 Minutes @ 177°C (350°F) Post Cure 16 Hours @ 232°C (450°F)
  • Elongation at Break, ASTM D412, Low Crosslink, Press Cure 10 Minutes @ 177°C (350°F) Post Cure 16 Hours @ 232°C (450°F)
  • Elongation at Break, ASTM D573, High Crosslink, Heat Aged
  • Elongation at Break, ASTM D573, Low Crosslink, Heat Aged
  • 100% Modulus, ASTM D412, Low Crosslink, Press Cure 10 Minutes @ 177°C (350°F) Post Cure 16 Hours @ 232°C (450°F)
  • 100% Modulus, ASTM D412, High Crosslink, Press Cure 10 Minutes @ 177°C (350°F) Post Cure 16 Hours @ 232°C (450°F)
  • Compression Set, ASTM D395 Method B, Plied Disc, High Crosslink
  • Compression Set, ASTM D395 Method B, Plied Disc, Low Crosslink
  • Compression Set, ASTM D395 Method B, Plied Disc, High Crosslink
  • Compression Set, ASTM D395 Method B, Plied Disc, Low Crosslink
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.