MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
BYK ADD-MAX® AS 38 Anti-static masterbatch, LLDPE based  (discontinued **)
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Fields of application: Anti-static masterbatch for olefinics

Examples: Thermoformed and injection molded PP or PE products such as containers and other packaging products. Other applications are films, sheets, tapes, yarns, fibers and household products.

Mode of action and advantages: ADD-VANCE AS 38 contains a high concentration of a highly effective synergistic blend of anti-static additives. The combination of internal anti-static agents used in this product reduces the surface resistance of olefinics.

Advantages: Immediate anti-static protection after production of the article; The balanced ratio of fast and controlled migrating anti-static additives does not only provide a rapid anti-static effect but also a prolonged protection against dust attraction and other inconveniences caused by electrostatic charging; Surface resistance of less than 1011 Ohm within 24 hours @ 1% dosing rate; Safe to use as a result of the food contact approved anti-static formulation; Excellent de-molding properties for injection molded products; Good cost economy; Non-sticking pellets, dust free dosing; and Safe and easy handling.

Regulations: ADD-VANCE AS 38 is very suitable for food packaging products as the active ingredients are in compliance with current food contact regulations

Former ADDCOMP product line, acquired by BYK.

Vendors:
Available Properties
  • Surface Resistance, 1% dosing rate
  • Processing Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Former Addcomp

Category Notes
none

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.