MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Covestro Bayhydrol® UH 2593/1 Polyurethane Coating
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings; Thermoset; Polyurethane, TS

Material Notes: Aliphatic, fatty acid-modified, anionic polyurethane dispersion. Binder for the formulation of water-reducible coatings and sealers for wood and wood materials.

Properties / Applications: The product was developed specifically for the formulation of one- and two-component wood coating systems. It is characterized by very good wet film transparency, high hardness and good black heel mark resistance. Post-curing of such coatings with Bayhydur® 305 or Bayhydur® 3100, for example, brings additional significant advantages and results in waterborne two-component coatings with even higher mechanical and chemical resistance. The mixing ratio of mill base to hardener solution is generally 10 : 1. The product is also suitable for use in a wide range of applications thanks to the combination of good application properties and good compatibility with cost-effective PAC dispersions. On account of the many potential co-reactants, compatibility testing should always be carried out.

Information provided by Covestro

Vendors:
Available Properties
  • Specific Gravity, DIN 51757
  • Volatiles, DIN EN ISO 3251, 1g/1h/125°C
  • Particle Size
  • pH, DIN ISO 976, 1:2.5 in demineralized water
  • Viscosity, DIN EN ISO 3219/A.3, D= approx. 100 s-1
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Covestro Deutschland AG, Bayer MaterialScience

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.