Bormed HE2581-PH is a high-density polyethylene intended for blow molding of products with high stiffness and very good environmental stress crack resistance (ESCR). Bormed HE2581-PH can as well be used to produce products via IBM or ISBM. Bormed HE2581-PH is recommended for bottles and containers up to 10 liters. Bormed HE2581-PH is designed for Pharmaceutical and diagnostic packaging, packaging for dialyze liquid, and containers for fine chemicals. Information provided by the Manufacturer. |