MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Total Lacqrene® 1240 Crystal Polystyrene  (discontinued **)
Categories: Polymer; Thermoplastic; Polystyrene (PS)

Material Notes: LACQRENE® 1240 is a high molecular weight crystal polystyrene, used in the dilution of high impact grades of polystyrene such as LACQRENE® 7240 or clear impact polystyrene such as Finaclear 520. LACQRENE® 1240 is designed to give excellent processing characteristics in combination with LACQRENE® 7240 and to give excellent dimension ability and improved mechanical performance over conventional crystals. When used pure, LACQRENE® 1240 is processed by extrusion and inline thermoforming or injection molding.

Application

Clear/colored cups, Objects by dilution with CLIPS/HIPS by extrusion thermoforming. Foamed polystyrene trays, Shower screens, Products with excellent mechanical properties obtained by injection molding.

Information provided provided by Total Petrochemicals.

Total Petrochemicals includes former Fina and Atofina plastics product lines.

Vendors:
Available Properties
  • Density, ISO 1183
  • Water Absorption, ISO 62
  • Linear Mold Shrinkage
  • Melt Flow, ISO 1133H
  • Hardness, Rockwell L, ISO 2039-2
  • Tensile Strength at Break, ISO 527-2
  • Elongation at Break, ISO 527-2
  • Tensile Modulus, ISO 527-2
  • Flexural Modulus, ISO 178
  • Charpy Impact Unnotched, ISO 179/1eU
  • Surface Resistivity per Square, ISO IEC93
  • Dielectric Strength
  • CTE, linear
  • Deflection Temperature at 0.46 MPa (66 psi), ISO 75-2B, Annealed
  • Deflection Temperature at 1.8 MPa (264 psi), ISO 75-2A, Unannealed
  • Vicat Softening Point, ISO 306B50, 50N (T° increase = 5°C/h)
  • Vicat Softening Point, ISO 306A50, 10N (T° increase = 50°C/h)
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Total Atofina

Category Notes
Plastic

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.