  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Skamol Group SICAL 78 Silicon Nitride-Bonded Silicon Carbide Brick
Categories: Ceramic; Carbide

Material Notes: Silicon nitride-bonded silicon carbide brick has the following characteristics:
  • Max. service temperature 1580°C (2876°F)
  • For sidewall lining of aluminum reduction cells
  • High thermal conductivity
  • Low porosity
  • Low thermal expansion
  • Low gas permeability
  • Outstanding abrasion and erosion resistance
  • High modulus of rupture
  • Superior resistance to metal penetration and attack
  • Extremely high crushing strength
  • Excellent oxidation resistance and resistance to corrosion

Information provided by Skamol.

Vendors:
Available Properties
  • Bulk Density, EN 993-1 1995
  • Porosity, EN 993-1 1995, Apparent
  • Permeability, EN 993-4 1995, nPm, Permeability to gases
  • Modulus of Rupture, EN 993-6: 1995
  • Compressive Strength, EN 993-5 1998
  • CTE, linear, ASTM C-372
  • Thermal Conductivity, SINTEF, Hot strip, Mean temp.
  • Thermal Conductivity, SINTEF, Hot strip, Mean temp.
  • Thermal Conductivity, SINTEF, Hot strip, Mean temp.
  • Maximum Service Temperature, Air
  • Al2O3 + Fe2O3 + CaO
  • Si3N4
  • SiC
  • Silicon, Si
  • SiO2 + Si2ON2
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

New MatWeb Services
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.