MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Solvay LTM® 110 series Ester Resin System
Categories: Polymer; Thermoset; Polyester, TS

Material Notes: Description: LTM110 series pregregs are high service temperature cyanate ester resin system capable of initial cure at temperatures as low as 70°C (158°F). After a suitable post-cure, the glass transition temperature can be increased to a maximum of 330°C (626°F), thus allowing components to withstand short duration thermal spikes up to this temperature. LTM110 series component pregregs have be specifically developed for applications where the best dimensional stability is required over a wide temperature range, and where tooling suitable for high temperature autoclave curing is not available.

Features & Benefits:

  • 3 days tack life at 21°C (70°F)
  • 6 months storage at -18°C (0°F)
  • 70°C (158°F) initial cure
  • Autoclave cure
  • Good dimensional stability and thermal durability up to 250°C (482°f) after post-cure
  • Maximum Tg of 330°C (626°F); can withstand thermal spikes to 330°C (626°F)
  • Inherently flame retardant, with low toxic gas and smoke generation
  • Good dielectric properties for radar transparency
Note 1: Material: LTM110/T300 (3k)-280 g/m2-4x4twill carbon fabric 55%Vf (2mm); Cure: 20 hrs at 70°C (158°F), 6 bar (90 psi); Post-cure: 0.5 hrs at 250°C (482°F)
Note 2: Material: LTM110/Quartz 581 fabric; Cure: 1 hr at 120°C (248°F), 6 bar (90 psi); Post-cure: 1 hr at 150°C (302°F)

Information provided by Cytec, subsequently acquired by Solvay.

Vendors:
Available Properties
  • Density, 20 hrs at 70°C + 2 hrs at 250°C
  • Storage Temperature
  • Tensile Strength, ASTM D3039, 0°C, Note 2
  • Tensile Strength, ASTM D3039, 0°C, Note 2
  • Tensile Modulus, ASTM D3039, 0°C, Note 2
  • Tensile Modulus, ASTM D3039, 0°C, Note 2
  • Flexural Strength, CRAG 200, Note 1
  • Flexural Strength, CRAG 200, Note 1
  • Flexural Strength, CRAG 200, Note 1
  • Flexural Strength, CRAG 200, Note 1
  • Flexural Strength, CRAG 200, Note 1
  • Flexural Strength, CRAG 200, Note 1
  • Flexural Strength, CRAG 200, Note 1
  • Flexural Strength, CRAG 200, Note 1
  • Flexural Strength, CRAG 200, Note 1
  • Flexural Strength, CRAG 200, Note 1
  • Flexural Strength, CRAG 200, Note 1
  • Flexural Strength, CRAG 200, Note 1
  • Flexural Strength, CRAG 200, Note 1
  • Flexural Strength, CRAG 200, Note 1
  • Flexural Modulus, CRAG 200, Note 1
  • Flexural Modulus, CRAG 200, Note 1
  • Flexural Modulus, CRAG 200, Note 1
  • Flexural Modulus, CRAG 200, Note 1
  • Flexural Modulus, CRAG 200, Note 1
  • Flexural Modulus, CRAG 200, Note 1
  • Flexural Modulus, CRAG 200, Note 1
  • Flexural Modulus, CRAG 200, Note 1
  • Flexural Modulus, CRAG 200, Note 1
  • Flexural Modulus, CRAG 200, Note 1
  • Flexural Modulus, CRAG 200, Note 1
  • Flexural Modulus, CRAG 200, Note 1
  • Flexural Modulus, CRAG 200, Note 1
  • Flexural Modulus, CRAG 200, Note 1
  • Compressive Strength, ASTM D3410, 0°C, Note 2
  • Compressive Strength, ASTM D3410, 0°C, Note 2
  • Compressive Modulus, ASTM D3410, 0°C, Note 2
  • Shear Modulus, ASTM D3518, 0°C, Note 2
  • Shear Modulus, ASTM D3518, 0°C, Note 2
  • Shear Strength, Interlaminar, Note 1, Aged 50 hrs at 300°C
  • Shear Strength, Interlaminar, Note 1, Aged 100 hrs at 300°C
  • Shear Strength, Interlaminar, Note 1, Aged 50 hrs at 250°C
  • Shear Strength, Interlaminar, Note 1, Aged 0 hrs at 250°C
  • Shear Strength, ASTM D3518, In-plane, Note 2
  • Shear Strength, ASTM D3518, In-plane, Note 2
  • Shear Strength, ASTM D2344, Interlaminar, Note 1
  • Shear Strength, ASTM D2344, Interlaminar, Note 1
  • Shear Strength, ASTM D2344, Interlaminar, Note 1
  • Shear Strength, ASTM D2344, Interlaminar, Note 1
  • Shear Strength, ASTM D2344, Interlaminar, Note 1
  • Shear Strength, ASTM D2344, Interlaminar, Note 1
  • Shear Strength, ASTM D2344, Interlaminar, Note 1
  • Shear Strength, ASTM D2344, Interlaminar, Note 1
  • Shear Strength, ASTM D2344, Interlaminar, Note 1
  • Shear Strength, ASTM D2344, Interlaminar, Note 1
  • Shear Strength, ASTM D2344, Interlaminar, Note 1
  • Shear Strength, ASTM D2344, Interlaminar, Note 1
  • Shear Strength, ASTM D2344, Interlaminar, Note 1
  • Shear Strength, ASTM D2344, Interlaminar, Note 1
  • Dielectric Constant, 20 hours at 70°C + 0.5 hrs at 250°C
  • Dielectric Constant, 20 hours at 70°C + 0.5 hrs at 250°C
  • Maximum Service Temperature, Air, thermal spikes
  • Glass Transition Temp, Tg, DMA E' onset, 16 hrs at 70°C
  • Glass Transition Temp, Tg, DMA E' onset, 2 hrs at 250°C
  • Glass Transition Temp, Tg, DMA E' onset, 0.5 hrs at 300°C
  • Shelf Life
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Solvay, former Rhodia Engineering Plastics

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.