MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Go Yen Chemical GYC TOTM
Categories: Other Engineering Material

Material Notes: GYC TOTM has low volatility and low migration and its electric resistivity and heat resistance are excellent.

Introduction: TOTM is produced by esterifying 2-Ethylhexanol and TrimelliticAnhydride. TOTM has low volatility and low migration and its electric resistivity and heat resistance are excellent. The wire and cable to which TOTM is applied in the process can pass USA s UL 62105°C class. TOTM’s migration and water extraction are lower than those of DIDP. To compare with DOP at the same flexibility, TOTM’s cold resistance is lower. With respect to PVC plastisol, under the condition of same flexibility, the viscosity of plastisol made with TOTM base is lower to that made with DIDP. As regards stability, since TOTM plastisol changes less than DOP, it is considered more stable than DOP.

Usage:

  • Wires & Cables
  • Leather & Clothes
  • Gloves
  • Shoes
  • Construction materials
  • PVC Plastisols

Information provided by Go Yen Chemical

Vendors:
Available Properties
  • Density, (20/20)
  • Viscosity
  • Molecular Weight
  • Acid Value, [mgKOH/g]
  • Volume Resistivity
  • Boiling Point
  • Flash Point
  • Refractive Index
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.