MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Bohler-Uddeholm UDDEHOLM RAMAX® LH Plastic Mold Steel  (discontinued **)
Categories: Metal; Ferrous Metal; Stainless Steel

Material Notes: Uddeholm Ramax LH is a new chromium alloyed stainless holder steel, which is supplied in the hardened and tempered condition.

RAMAX® LH is characterized by:

  • Excellent machinability
  • Good corrosion resistance
  • Good hardenability
  • Uniform hardness in all directions
  • Good indentation resistance
Applications
  • Holders/bolsters for plastic moulds
  • Plastic and rubber moulds with low requirements on polishability
  • Die and calibers for plastic extrusion
  • Constructional parts

Vendors:
Available Properties
  • Density, hardened and tempered to 350 HB
  • Hardness, Brinell, Hardened and tempered (Delivery condition)
  • Hardness, Brinell
  • Tensile Strength, Ultimate, (hardened to 302 HB)
  • Tensile Strength, Ultimate, (hardened to 302 HB)
  • Tensile Strength, Yield, 68°F (hardened to 302 HB)
  • Tensile Strength, Yield, hardened to 302 HB
  • Elongation at Break, (hardened to 302 HB)
  • Elongation at Break, hardened to 302 HB
  • Reduction of Area, hardened to 302 HB
  • Reduction of Area, hardened to 302 HB
  • Modulus of Elasticity, 68°F, (hardened and tempered to 302 HB)
  • Modulus of Elasticity, hardened and tempered to 302 HB
  • Impact Test, unnotched
  • CTE, linear, hardened and tempered to 302 HB
  • Specific Heat Capacity, hardened and tempered to 302 HB
  • Thermal Conductivity, hardened and tempered to 302 HB
  • Carbon, C
  • Chromium, Cr
  • Iron, Fe, as balance
  • Manganese, Mn
  • Molybdenum, Mo
  • Nickel, Ni
  • Silicon, Si
  • Sulfur, S
  • Vanadium, V
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

New MatWeb Services
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.