MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Rubaloy Rubaloy S NBR / PVC
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Product Information: Rubaloy - S is a low hardness NBR / PVC blend in the polymer ratio of 3:2 with special additives of Polymeric Plasticizers, Internal Lubricants, Stabilizers and Anti-Oxidants for easy compounding/blending. Due to its low hardness as compared to other NBR / PVC grades it is highly recommended for use in expanded Micro Cellular Sponge products. Also, for use in low hardness printing rolls and high oil, ozone and flex-crack resistant products.

Processing Characteristics: Easily processable on conventional rubber processing machines. Very quick filler and plastic absorption. Warm mixing mill roll or processing chamber recommended for best results. Can easily withstand elevated compounding temperatures upto 140°C.

Applications: Very light weight micro-cellular open and closed celled and expanded foam / sponge products like footwear, insulation sheets, sports goods, toys, sound proofing sheets, oil and ozone resistant sheets and molded articles, health-care products, lining, printing rolls, profiles, etc. Also, molded goods, soft extruded profiles, etc.

Information provided by Rubaloy™

Vendors:
Available Properties
  • Specific Gravity
  • Mooney Viscosity, ML 1+4
  • Hardness, Shore A
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.