Product Description: MBTS (Benzothiazyl Disulfide) is a non-staining, primary thiazole accelerator for use in natural and synthetic rubbers. It is very active at temperatures above 280°F. Activation requires the addition of zinc oxide, a fatty acid and sulfur for cure development. Secondary accelerators used in conjunction with MBTS such as aldehyde amines, dithiocarbamates, guanidines, and thiurams will increase cure rates. MBTS is also used as a retarder in polychloroprene cure systems, as well as a retarder for peroxide cures. Blends of MBTS and BBTS are often employed in tire vulcanization cure systems. MBTS is a safe processing accelerator, but increased scorch resistance can be obtained with the addition of Retarder PX, Retarder AK, or Retarder SAFE.Information provided by Akrochem Corporation |