MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Celanese Celcon® M140 POM, Unfilled
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM)

Material Notes: Celcon« acetal copolymer grade M140 is a moderately high flow general purpose injection molding grade. It is designed for use in applications requiring some enhanced flow characteristics over the standard Celcon« M90 material.

Information provided by Celanese

Vendors:
Available Properties
  • Specific Gravity, ASTM D792
  • Density, ISO 1183
  • Density of Compound
  • Moisture Absorption, ISO 62, 23°C/50%RH
  • Water Absorption at Saturation, ISO 62
  • Linear Mold Shrinkage, Flow, ISO 294-4
  • Linear Mold Shrinkage, Flow, ASTM D955
  • Linear Mold Shrinkage, Transverse, ISO 294-4
  • Linear Mold Shrinkage, Transverse, ASTM D955
  • Melt Flow, ISO 1133, [cm3/10min]
  • Tensile Strength, Yield, ASTM D638
  • Tensile Strength, Yield, ISO 527-2/1A, 50mm/min
  • Tensile Strength, Yield, ASTM D638
  • Tensile Strength, Yield, ASTM D638
  • Elongation at Yield, ISO 527-2/1A, 50mm/min
  • Tensile Modulus, ISO 527-2/1A, 50mm/min
  • Flexural Modulus, ASTM D790
  • Flexural Modulus, ISO 178
  • Flexural Modulus, ASTM D790
  • Flexural Modulus, ASTM D790
  • Izod Impact, Notched, ASTM D256
  • Izod Impact, Notched, ASTM D256
  • Izod Impact, Notched (ISO), ISO 180/1A
  • Charpy Impact, Notched, ISO 179/1eA
  • Tensile Creep Modulus, 1 hour, ISO 899-1
  • Tensile Creep Modulus, 1000 hours, ISO 899-1
  • CTE, linear, Parallel to Flow, ISO 11359-2
  • CTE, linear, Transverse to Flow, ISO 11359-2
  • Specific Heat Capacity
  • Thermal Conductivity
  • Melting Point, ISO 11357-1,-2,-3, 10°C/min
  • Deflection Temperature at 0.46 MPa (66 psi), ISO 75-1, -2
  • Deflection Temperature at 1.8 MPa (264 psi), ISO 75-1, -2
  • Deflection Temperature at 1.8 MPa (264 psi), ASTM D648
  • Processing Temperature, cavity
  • Processing Temperature, hot runner
  • Zone 1
  • Zone 2
  • Zone 3
  • Zone 4
  • Die Temperature
  • Melt Temperature
  • Drying Temperature
  • Dry Time
  • Injection Pressure
  • Hold Pressure
  • Back Pressure
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Ticona, Celanese Corporation

Category Notes
Plastic
POM, Polyoxymethylene

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.