MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
SABIC SABIC® HDPE F0863 PE (Global)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: SABIC® HDPE F0863 resin is a homopolymer with a very high density manufactured by gas phase technology. The grade offers high stiffness, high temperature resistance, low water vapor transmission and a very low gel level. Because of the linear character it is advisable to use the material in combination with extrusion coating LDPE grades like SABIC® LDPE 2005EC in order to improve extrusion coating process ability (motor load and Neck In). SABIC® HDPE F0863 is typically used for food packaging, release paper and photographic paper. Film properties have been measured at cast film of 25 µm. Water vapor permeability at 38 °C and 100 % RH per 24 h. Oxygen permeability at 23 °C and 0 % RH per 24 h. This product is not intended for and must not be used in any pharmaceutical/medical applications.

Information provided by SABIC

Vendors:
Available Properties
  • Density, ASTM D1505
  • Water Vapor Transmission, SABIC method
  • Oxygen Transmission Rate, SABIC method
  • Melt Flow, ISO 1133
  • Neck In, SABIC method, Measured on pilot line at 200 m/min, 300 °C, 10 g/m², airgap 300 mm
  • Film Tensile Strength at Yield, MD, ISO 527-3
  • Film Tensile Strength at Yield, TD, ISO 527-3
  • Film Elongation at Break, MD, ISO 527-3
  • Film Elongation at Break, TD, ISO 527-3
  • Tensile Modulus, ISO 527-3, TD
  • Tensile Modulus, ISO 527-3, MD
  • Film Tensile Strength at Break, MD, ISO 527-3
  • Film Tensile Strength at Break, TD, ISO 527-3
  • Heat of Fusion, DIN 53765
  • Melting Point, DIN 53765
  • Vicat Softening Point, ISO 306, at 10 N (VST/A)
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Saudi Basic Industries Corporation; SABIC Innovative Plastics (GE Plastics)

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.