MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
ITW Chockfast® Red Epoxy Grouting Compound
Categories: Polymer; Thermoset; Epoxy

Material Notes: CHOCKFAST Red is a three-component, high strength, 100% solids, epoxy grouting compound used to grout large machinery and to support soleplates in all types of foundations. CHOCKFAST Red has an extremely high compressive strength. This along with negligible shrinkage makes it ideal for installing critically aligned machinery within very close tolerances.

USE & BENEFITS: CHOCKFAST Red has the following advantages when compared to conventional cement-based non-shrink grouts: • Impervious to oil • Cures at least three times as quickly • No mixing ratios to measure • Grouts machinery in final aligned position • High physical strength • High impact strength • Resistance to many more chemicals • Strong bond to metal and concrete • Unaffected by weathering and freeze / thaw cycling • Stated physical properties assured • Superior resistance to fatigue.

Information provided by ITW Performance Polymers.

Vendors:
Available Properties
  • Specific Gravity
  • Tensile Strength, ASTM D638
  • Flexural Strength, ASTM C580
  • Flexural Modulus, ASTM C580
  • Compressive Strength, ASTM C579 MOD
  • Compressive Modulus, ASTM C579 MOD
  • Izod Impact, Notched, ASTM D256
  • CTE, linear, ASTM D696
  • Shrinkage, ASTM D2566, Not measurable
  • Cure Time, approximate
  • Cure Time, approximate
  • Cure Time, approximate
  • Cure Time, approximate
  • Pot Life, Approximate
  • Shelf Life, In dry storage
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.