MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Chesterton 690 FG Lubricant
Categories: Fluid; Lubricant

Material Notes: Chesterton® 690 FG Lubricant is a high-quality, cost-effective penetrating lubricant. Used in food processing, beverage and pharmaceutical plants, 690 FG Lubricant can go where few products have gone before. The product's ultra-high purity makes it applicable wherever incidental food contact can occur, and its non-staining features allow it to be used wherever cleanliness is critical. 690 FG Lubricant has excellent capillary actions: It effectively creeps between close tolerances and provides lubrication to otherwise oil-starved areas. Its smooth lubricating film stops noise and reduces friction and wear on all types of moving equipment, thereby saving costly break downs and shutdowns as well as the costs for replacement parts.

Features:

  • Conforms to FDA standards (CFR 178.3620, 178.3570)
  • Clear, colorless, odorless
  • High flash point
  • Environmentally friendly aerosol packaging
  • NSF H1 - Registration number 133969 (bulk) and 133933 (aerosol)

Benefits:

  • Save production time
  • Reduce labor costs
  • Reduce maintenance costs
  • Save the cost of replacement parts
  • Prolong the life of machinery and parts
  • Significantly reduce power consumption
  • Pinpoint spray means no product waste
  • Save excess product costs
  • Safe to use; easy to use

Applications: 690 FG Lubricant is made of ingredients conforming to applicable FDA standards for incidental contact areas. 690 FG Lubricant is suitable for use in federally inspected meat and poultry plants. It is also used where a clean, nonstaining lubricant is required, including textile and pulp & paper plants. Suggested uses include all types of processing equipment where incidental food contact can occur

  • Cannign and bottling machinery
  • Carton-filling machinery
  • Paste and sauce fillers
  • Meatpacking equipment
  • Fruit feeders
  • Bakery equipment
  • Cams and rotary fillers
  • Mixers
  • Stainless steel pumps
  • Metering pumps/valves
  • Pneumatic equipment
  • Steel conveyor belts and rollers
  • Chain drives
  • Pistons, rollers, bearings

Information provided by Chesterton

Vendors:
Available Properties
  • Specific Gravity
  • Kinematic Viscosity at 40°C (104°F), ASTM D445, DIN 51 561
  • Coefficient of Friction, ASTM D43233, Falex
  • Four Ball Extreme Pressure, Load Wear Index, ASTM D2266, DIN 51 350
  • Four Ball Extreme Pressure, Weld Load, ASTM D2266, DIN 51 350
  • Four Ball Wear, ASTM D2266, DIN 51 350
  • Falex Load Test, ASTM D43233, Weld Load
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Pour Point, ASTM D97, ISO 3016
  • Flash Point, ASTM D92, ISO 2592
  • FDA, See notes for details.
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.